SA285 Grade C is a pressure vessel plates in carbon steel, low and intermediate tensile strength. SA285 Grade C should be made by killed; semi killed, capped or rimmed steel practice at the producer option to be used for fusion welded pressure vessels.
 
The max thickness of SA285 Grade C should under 50mm because of the reason of internal soundness.

 
Gangsteel is large agent in HBIS and cooperated with Wuyang Iron and steel co.,ltd to export high quality steel plate. For the competitive price in SA285 Grade C, please contact us by email.
 

SA285 Grade C steel Chemical requirement in Product analysis

C %
Mn %
P %
S %
SI %
0.28
0.98
0.035
0.035
0.08-0.45

 
 

Mechanical Property SA285 Grade C

Mechanical Property SA285 Grade C
SA285 Grade C
Tensile strength, kis [MPa]
Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %
380-515
205
27

 
 