SA285 Gr.A,ASME SA285 Gr.CA,SA285 Gr.A steel plate

2013年8月26日 by admin

 

ASME SA285 standard specification for pressure vessel plates, carbon steel, low- and intermediate-tensile strength, normally supplied in the as-rolled condition. The plates may be ordered normalized or stress relieved, or both.

 

Our plates including SA285 Grade A come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S57 | S57.1 | S58 | S58.1 |S3 |S4

 

Dimension: Thickness: 6MM to 300MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm

Gangsteel is specialized in supplying ASME SA285 steel plate in SA285 grade A. For more information of SA285 grade A steel plates, please check them in following:

 

SA285 grade A Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

SA285 grade A

0.17

0.08-0.45

0.98

0.035

0.035

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Grade

 

SA285 grade A Mechanical Property

Thickness

Yield

Tensile

Elongation

SA285 grade A

mm

Min Mpa

Mpa

Min  %

6-50

165

310-450

30%

50-200

165

310-450

27%

Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of SA285 grade A

Europe

British

Germany

Spain

Italy

Sweden

India

Japan

P235GH

161 Gr.360/164 Gr.360

HI

A 37 RCI

Fe 60-1KW

 

 

SPV 24

Related Grade: SA285 grade B | SA285 grade C

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASME SA285, ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about SA285 Gr.A or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

Tags: SA285 Gr.A  SA285 Grade A  ASME SA285 Gr.A  SA285 Gr.A steel plate  

0 Comments, 0 Trackbacks