New Products /back


ASME SA302 Grade B,SA302 Gr. B steel,SA302 GRB steel plate

2013年9月4日 by admin

Adopt standard: ASME SA302

 

Sell steel grade: SA302 Grade A ,SA302 Grade B,SA302 Grade C, SA302 Grade D steel grade

 

SA302 Grade B steel plate

 

SA302 Grade B steel plates standard specification for pressure vessel plates in alloy steel, manganese molybdenum 

and manganese-molybdenum-nickel.

 

SA302 Grade B steel grade is min yield strength in 310Mpa. Gangsteel also supply the Ultrasonic test in thickness in

 A435/A435M, A577/577Mand A578/A578Mto promise the perfect quality in long cooperation.

 

SA302 Grade B steel plate shall be normally supplied in the as-rolled condition. Plates may be ordered normalized 

or stress relieved, or both. If SA302 Grade B steel plate is above 50mmin thickness shall be normalized.

 

Gangsteel supplied SA302 Grade B to export many years. We have contacted the technical department of HBIS wuyang mill,

 from ingot or billet steel, to hot rolled process and normalized treatment, each item in manufacture, Gangsteel have the person to

 tract for our customers in order to in the fastest delivery time.

 

SA302 Grade B steel Tensile Requirements:

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

25mm or under
25mm - 50mm
over 50mm

0.20
0.23
0.25

Heat Analysis

Product Analysis

1.15-1.50

1.07-1.62

Heat Analysis

Product Analysis

0.15-0.40

0.13-0.45

 

All thick

 

0.035

 

 

Molybdenum max

%

Nickel max

%

Phosphorus

%

 

 

Heat Analysis

Product Analysis

0.45-0.60

0.41-0.64

Heat Analysis

Product Analysis

…..

……

All thick

0.035

 

SA302 Gr.B steel Tensile Requirements:

Mechanical Property of SA302 Gr.B steel plate

SA302 Gr.B

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

80-100 [550-690]
50 [345]

15

18

 

If you have any need in SA302 Grade B steel, please feel free to contact us soon by email or calling. 

Tags: SA302 Grade B  SA302 Gr.B  Sa302 GrB  SA302 Gr.B steel plate  ASME SA302 Gr.B  ASME SA302 Gr.B  ASME SA302 Grade B  SA302 GRB supplier  SA302 Grade B steel grade  SA302 Gr.B price  