SA302 Gr.C,SA302 Gr.C steel,SA302 Gr.C steel plate

 

Adopt standard: ASME SA302

Sell steel grade: SA302 Grade A, SA302 Grade B, SA302 Grade C, SA302 Gr.C steel grade

 

 

SA302 Gr.C steel plates shall be killed and conform to the fine grain size requirement of specification A 20/A 20M.


SA302 Gr.C is Mn- Mo-Ni alloy steel grade, the same with SA302 Grade C. SA302 Gr.D min yield strength is 345Mpa.


SA302 Gr.C also has the supplementary requirements in S1, S2, S3, S4.1, S5, S7, S8, S9, S11, S12, S17. and HIC test.

 

Our plates including SA302 Grade C come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

Gangsteel supplied SA302 Gr.C to export many years. We have contacted the technical department of wuyang mill, from ingot or billet steel, to hot rolled process and normalized treatment, each item in manufacture, Gangsteel have the person to tract for our customers in order to in the fastest delivery time.

 

SA302 Gr.C steel Chemical Requirements:

Carbon, max

%

Manganese, max

%

Silicon, max

%

Sulfur max

%

25mm or under
25mm - 50mm
over 50mm

0.20
0.23
0.25

Heat Analysis

Product Analysis

1.15-1.50

1.07-1.62

Heat Analysis

Product Analysis

0.15-0.40

0.13-0.45

 

All thick

 

0.035

 

 

Molybdenum max

%

Nickel  max

%

Phosphorus

%

 

 

Heat Analysis

Product Analysis

0.45-0.60

0.41-0.64

Heat Analysis

Product Analysis

0.40-0.70

0.37-073

All thick

0.035

 

SA302 Gr.C steel Tensile Requirements:

Mechanical Property of SA302 Gr.C steel plate

SA302 Gr.C

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

80-100 [550-690]
50 [345]

17

20

 