New Products /back


ASME SA302 Grade C, SA302 Grade C steel, SA302 Grade C steel plate

2013年9月4日 by admin

Adopt standard: ASME SA302

Sell steel grade: SA302 Grade A,SA302 Grade B,SA302 Grade C, SA302 Grade D steel grade
 
SA302 Grade C steel plates shall be killed and conform to the fine grain size requirement of specification A 20/A 20M.

SA302 Grade C is Mn- Mo-Ni alloy steel grade, the same with SA302 Grade D. SA302 Grade C min yield strength is 345Mpa. When normalized SA302 Grade C in thickness 100mm or over in thickness, the cooling rate maybe accelerated by air blasting or liquid quenching to obtain mechanical properties comparable to those developed by normalizing plates in the lesser thickness.
 
Gangsteel supplied SA302 Grade C to export many years. We have contacted the technical department of wuyang mill, from ingot or billet steel, to hot rolled process and normalized treatment, each item in manufacture, Gangsteel have the person to tract for our customers in order to in the fastest delivery time.
 
 
SA302 Grade C steel Chemical Requirements:

Carbon, max
%
Manganese, max
%
Silicon, max
%
Sulfur max
%
25mm or under
25mm - 50mm
over 50mm
0.20
0.23
0.25
Heat Analysis
Product Analysis
1.15-1.50
1.07-1.62
Heat Analysis
Product Analysis
0.15-0.40
0.13-0.45
 
All thick
 
0.035
 
 
Molybdenum max
%
Nickel max
%
Phosphorus
%
 
 
Heat Analysis
Product Analysis
0.45-0.60
0.41-0.64
Heat Analysis
Product Analysis
0.40-0.70
0.37-073
All thick
0.035

 
SA302 Grade C steel Tensile Requirements:
 

Mechanical Property of SA302 Grade C steel plate
SA302 Grade C
Tensile strength, kis [MPa]
Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %
80-100 [550-690]
50 [345]
17
20

 
If you have any need in SA302 Grade C steel, please feel free to contact us soon by email or calling.
 