New Products /back


SA514 Grade P,SA514 Grade P steel,SA514 Grade P steel plate

2013年8月28日 by admin

 Adopt Standard: ASME SA517

 

SA514 Grade P is for high yield strength, quenched and tempered alloy steel plate of structural quality in thickness of 150mm and under intended primarily for use in welded bridges and other structures.
 

The max thickness of SA514 Grade P is 150mm. in the heat treatment, SA514 Grade P shall be heat treatment by the mill to conform to the tensile and hardness requirements by heating to not less 900 degree and quenching in water or oil, tempering at not less 620 degree.

 

Gangsteel is the large agent in HBIS Wuyang mill and we have exported SA514 Grade P to be used in oil platform project.

 

Our plates including SA514 Gr.P come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.


SA514 Grade P steel Chemical requirement in Heat analysis:

C %

Mn %

P %

S %

SI %

Ni %

Cr %

0.12-0.21

0.45-0.70

0.035

0.035

0.20-0.35

1.20-1.50

0.85-1.20

Mo %

B %

V %

Ti %

Zr %

Cu %

Co %

0.45-0.60

0.001-0.005

 

 

 

 

 

 
Mechanical Property SA514 Grade P:

Mechanical Property SA514 Grade P

SA517 Grade P

20mm and under

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]

Elongation in under [50mm], min, %

Brinell Hardness Number

20mm-65mm

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %

65mm-150mm

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %

20mm and under

760-895

690

18

235-293

20mm-65mm

760-895

690

18

65mm-150mm

690-895

620

16

Shipbuilding steel plate| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate

  

Related Grade: A514 Grade A|A514 Grade B|A514 Grade C|A514 Grade E|A514 Grade F|A514 Grade H|A514Grade J|A514 Grade K|A514 Grade M|A514 Grade P|A514 Grade Q|A514 Grade R|A514Grade S|A514 Grade T

 

To find more about SA514 Gr M or other boiler and pressure vessel steel grade, and to receive competitive price, please feel free to CLICK HERE to contact us.

 

Tags: SA514 Grade P  SA514 Gr.P  ASME SA514 Gr.P  SA514 Grade P steel  SA514 Grade P steel plate  

0 Comments, 0 Trackbacks