SA514 Grade S steel plate
2013年8月12日 by admin
SA514 Grade S,SA514 Grade S steel,SA514 Grade S steel plate
Adopt Standard: ASME SA514, ASTM A514
SA514 Grade S is for high yield strength, quenched and tempered alloy steel plate of structural quality in thickness of 65mm and under intended primarily for use in welded bridges and other structures.
The max thickness of SA514 Grade S is 65mm. in the heat treatment, SA514 Grade S shall be heat treatment by the mill to conform to the tensile and hardness requirements by heating to not less 900 degree and quenching in water or oil, tempering at not less 620 degree.
Gangsteel is the large agent in HBIS Wuyang mill and we have exported SA514 Grade S to be used in oil platform project. Our plates including SA514 Gr.S come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.
SA514 Grade S steel Chemical requirement in Heat analysis:
C % | Mn % | P % | S % | SI % | Ni % | Cr % |
0.11-0.21 | 1.10-1.50 | 0.035 | 0.035 | 0.15-0.45 | | . |
Mo % | B % | V % | Ti % | Zr % | Cu % | Nb % |
0.10-0.60 | 0.001-0.005 | 0.06 | | | | 0.06 |
Mechanical Property SA514 Grade S:
Mechanical Property SA514 Grade S | SA514 Grade S |
20mm and under Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in under [50mm], min, % Brinell Hardness Number 20mm-65mm Tensile strength, kis [MPa] Yield strength, min, kis [MPa] | 20mm and under 760-895 690 18 235-293 20mm-65mm 760-895 690 18 |
Shipbuilding steel plate| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate
Related Grade: A514 Grade A|A514 Grade B|A514 Grade C|A514 Grade E|A514 Grade F|A514 Grade H|A514Grade J|A514 Grade K|A514 Grade M|A514 Grade P|A514 Grade Q|A514 Grade R|A514Grade S|A514 Grade T
To find more about SA514 Gr B or other boiler and pressure vessel steel grade, and to receive competitive price, please feel free to CLICK HERE to contact us.