SA515/SA515M specification covers carbon-silicon steel plates primarily for intermediate and higher temperature service in welded boilers and other pressure vessels projects.
SA515 Gr.70 steel tensile strength is 485Mpa to 620Mpa and the yield strength is min 260Mpa.
About the thickness of SA515 Gr.70, Gangsteel maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is 300mm. the delivery station is UT test, normalized and have to use the ingot to produce it.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is 300mm. the delivery station is UT test, normalized and have to use the ingot to produce it.
SA515 Gr.70 heat treatment, if SA515 Gr.70 steel thick in 50mm or under this thickness, SA515 Gr.70 normalized supplied in the as-rolled condition. If our customer requirement, we also could do normalized. If SA515 Gr.70 thicknesses above 50mm, this plate shall be normalized..
Our Gangsteel is specialized in super thick steel plate, and we also have much experience about A HIC test. We could provide DNV, ABS, LR ,BV,CCS,GL,CE mark certificate in our super thickness to promise our steel quality. We sincerely invite our new and old customer come to visit our mill for our long steel business.
SA515 Gr.70 Chemical requirements :
Carbon, max | % | Manganese, max | % | Silicon, max | % | |
25mm or under 25mm - 50mm 50mm- 100mm 100mm- 200mm over 200mm | 0.31 0.33 0.35 0.35 0.35 | Heat Analysis Product Analysis | 1.20 1.30 | Heat Analysis Product Analysis | 0.15-0.40 0.13-0.45 | |
Phosphorus max | % | Sulfur max | % | | | |
All thickness | 0.035 | All thickness | 0.035 | | |
SA515 Gr.70 Tensile requirements
Mechanical Property | SA515 Gr.70 |
Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in 8 in. [200 mm], min, % Elongation in 2 in. [50 mm], min, % | 70-90 [485-620] 38 [260] 17 21 |
If any need in SA515 Gr.70,SA515gr70,SA515 gr 70 steel plate, please feel free to contact our Gangsteel, we will give our competitive price, faster delivery and the best quality.