SA515 Grade 60, SA515 Gr. 60 steel plate
2013年8月27日 by admin
Adopt Standard: ASME SA515
SA515/SA515M specification covers carbon-silicon steel plates primarily for intermediate and higher temperature service in welded boilers and other pressure vessels projects.
SA515 Grade 60 steel tensile strength is 415Mpa to 550Mpa and the yield strength is min 415Mpa.
About the thickness of A515 Gr 60, Gangsteel maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is 300mm. the delivery station is UT test, normalized and have to use the ingot to produce it.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is 300mm. the delivery station is UT test, normalized and have to use the ingot to produce it.
SA515 Grade 60 heat treatment, if SA515 Grade 60 steel thick in 50mm or under this thickness, SA515 Grade 60 normalized supplied in the as-rolled condition. If our customer requirement, we also could do normalized. If SA515 Grade 60 thicknesses above 50mm, this plate shall be normalized..
Our Gangsteel is specialized in super thick steel plate, and we also have much experience about A HIC test. We could provide DNV, ABS, LR ,BV,CCS,GL,CE mark certificate in our super thickness to promise our steel quality. We sincerely invite our new and old customer come to visit our mill for our long steel business.
SA515 Grade 60 Chemical requirements:
Carbon, max | % | Manganese, max | % | Silicon, max | % | |
25mm or under 25mm - 50mm 50mm- 100mm 100mm- 200mm over 200mm | 0.24 0.27 0.29 0.31 0.31 | Heat Analysis Product Analysis | 0.90 0.98 | Heat Analysis Product Analysis | 0.15-0.40 0.13-0.45 | |
Phosphorus max | % | Sulfur max | % | | | |
All thickness | 0.035 | All thickness | 0.035 | | |
SA515 Grade 60 Tensile requirements:
Mechanical Property | SA515 Grade 60 |
Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in 8 in. [200 mm], min, % Elongation in 2 in. [50 mm], min, % | 60-80 [415-550] 32 [220] 21 25 |
Equivalent steel grade of SA516 grade 60 | |||||||
| | | | | | | |
| | E St E315 | | Fe 460-2-KG | SS29,12,01 | | |
Related Grade: SA516 Grade 55 | SA516 Grade 65 |SA516 grade 70
If any need in SA515 Grade 60,a515gr60,a515 gr 60 steel plate, please feel free to contact our Gangsteel, we will give our competitive price, faster delivery and the best quality.
Tags: SA515 Grade 60 SA515 Gr.60 SA515 Grade 60 supplier SA515 Grade 60 steel plate