SA517 Grade A,SA517 Grade A steel,SA517 Grade A,steel plate

2011年6月10日 by admin

 

SA517 Grade A,SA517 Grade A steel,SA517 Grade A,steel plate
 
Adopt Standard: ASME SA517
Gang steel grade: SA517 Grade A
SA517 Grade A steel plate
SA517 Grade A is a high strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure vessels.
 
The maximum thickness of plate,
grade A and grade B are 32mm: Grade H and grade S are 50mm: grade P is 100mm: Grade F, is 65mm: Grade E and grade Q are 150mm in thickness

 
Gangsteel is a large agent in HBIS and cooperated with Wuyang Iron and steel co.,ltd to export high quality and super thickness steel plate. For the competitive price in SA517 Grade A, please contact us by email.

SA517 Grade A steel Chemical requirement in Product analysis
 

C %
Mn %
P %
S %
SI %
Ni %
Cr %
0.13-0.23
0.74-1.20
0.035
0.035
0.34-0.86
 
0.46-0.84
Mo %
B %
V %
Ti %
Zr %
Cu %
Co %
0.15-0.31
0.025
 
 
0.04-0.16
 
 

 

Mechanical Property SA517 Grade A
 

Mechanical Property SA517 Grade A
SA517 Grade A
65mm and under
Tensile strength, kis [MPa]
Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %
65mm-100mm
Tensile strength, kis [MPa]
Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %
65mm and under
795-930
690
16
65mm-100mm
725-930
620
14

 
If you want to know price in SA517 Grade A from our Gangsteel, please inquiry us by email or calling.
 