SA517 Grade S steel plate

2013年8月12日 by admin

 SA517 Gr.S,SA517 Gr.S steel,SA517 Gr.S steel plate

 Adopt Standard: ASME SA517

 
SA517 Gr.S is a high strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure vessels.

 

The maximum thickness of plate, grade A and grade B are 32mm: Grade H and grade S are 50mm: grade P is 100mm: Grade F, is 65mm: Grade E and grade Q are 150mm in thickness

Gangsteel is a large agent in HBIS and cooperated with Wuyang Iron and steel co.,ltd to export high quality and super thickness steel plate.  Our plates including SA517 Gr.S come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.


SA517 Gr.S steel Chemical requirement in Product analysis:

C %

Mn %

P %

S %

SI %

Ni %

Cr %

0.10-0.22

1.02-1.62

0.035

0.035

0.13-0.45

 

 

Mo %

B %

V %

Ti %

Zr %

Cu %

Co %

0.10-0.384

 

0

0.07

 

 

0.07

 
Mechanical Property SA517 Gr.S:

Mechanical Property SA517 Gr.S

SA517 Gr.S

65mm and under

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]

Elongation in under [50mm], min, %

65mm-100mm

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %

65mm and under

795-930

690

16

65mm-100mm

725-930

620

14

Shipbuilding steel plate| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate

  

Related Grade: SA517 Grade A|SA517 grade B| SA517 grade E| SA517 grade F| SA517 grade H| SA517 grade P| SA517 grade Q|SA517 grade S

 

To find more about SA517 Gr S or other boiler and pressure vessel steel grade, and to receive competitive price, please feel free to CLICK HERE to contact us.

Tags: SA517 Gr.S  SA517 Gr.S steel  SA517 Gr.S steel plate  SA517 Grade S  SA517 GRS  ASME SA517  SA517 Gr.S price  

0 Comments, 0 Trackbacks