New Products /back


A203 grade D,A203 Gr D,ASTM A203GrD,A203 Grade D steel

2011年4月14日 by admin

A203 grade D,A203 Gr D,A203GrD,A203 Grade D steel,A203 Gr D steel plate.

 

Adopt standard: ASTM A 203/A 203M-01

Gangsteel steel grade: A203 Grade A,A203 Grade B,A203 Grade D,A203 Grade E and A203 Grade F steel.

 

A203 Grade D steel plate

A203 Grade D steel grade is a nickel alloy steel plate in welded pressure vessels. For this A203 Grade D is max thickness in 100mm and the element of nickel is 3.25% to be used in manufacturing pressure vessel and boilers.

 

A203 Grade D steel plate, in yield of 255Mpa , Tensile in 450Mpa. In fact, The A203 Gr.A and A203 Gr.D are the same in mechanical property. But the A203 Gr.D nickel is 3.25% , A 203 Gr. A nickel 2.25%.

Gangsteel has much experience exporting boiler plate in A203 Grade D to factory mill many years. Besides that, Gangsteel has a specialized person who worked at production line of steel, to arrange our customer goods to produce as early as possible. Gangsteel welcomes our customer to visit in our mill.

Besides that, Gangsteel has a person who worked at production line of steel, to arrange our customer’s goods to produce as early as possible. Gangsteel welcomes our customer to visit in our mill.

A203 Grade D steel Chemical Requirements In product analysis under 50mm thickness

Element

A203 Grade A  Max %

C

0.17

Si

0.13-0.45

Mn

0.78-0.88

P

0.035

S

0.035

Ni

3.18-3.82

 

 

A203 Grade D steel Tensile Requirements

Mechanical Property of A203 Grade D steel plate

A203 Grade D

Tensile strength, kis [MPa]

50mm or under

Over 50mm

Yield strength, min, kis [MPa]

50mm or under

Over 50mm
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

Tensile strength, kis [MPa]

65-85 [450-585]
65-85 [450-585]

Yield strength, min, kis [MPa]

37 [255]

37 [255]

19

23

 

If you have any need in A203 Grade D, please contact Gangsteel soon by email or calling.

A203,A203Grade D,A203 grade D,A203 Gr D,A203GrD,A203 Grade D steel,A203 Gr D steel plate. Pressure steel plate.

 

 

Tags: A203 grade D  A203 Gr D  ASTM A203GrD  A203 Grade D steel  

0 Comments, 0 Trackbacks