A387 Grade 9 Class 1 is a chromium molybdenum alloy steel plates intended primarily for welded boiler and pressure vessels designed of elevated temperature service.

 

Each grade except grade 21L,Grade 22L,Grade 91 and Grade 911 is available in two classes of tensile strength levels. Grade 91 and Grade 911 are available only as Class 2.

A387 Grade 9 Class 1 max thickness of plates is limited only by the capacity of the composition to meet specified mechanical property requirements.

Gangsteel is a large agent in HBIS and cooperated with Wuyang Iron and steel co.,ltd to export high quality and super thickness steel plate. For the competitive price in A387 Grade 9 Class 1, please contact us by email.


A387 Grade 9 Class 1 steel Chemical requirement in Product analysis:

C %

Mn %

P %

S %

SI %

Cr %

Mo %

0.15

0.25-0.66

0.030

0.030

1.05

7.90-10.10

0.85-1.10

Ni %

V %

Nb %

B %

Nitrogen

AL %

Tungsten

 

 

 

 

 

 

 


Mechanical Property A387 Grade 9 Class 1:

Mechanical Property A387 Grade 9 Class 1

A387 Grade 9 Class 1

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [200mm], min, %

Elongation in under [50mm], min, %

415-585

205

….

18

 