A387 Gr5 Cl.2,A387 Grade 5 Class 2, A387 Gr5 Cl2 steel plate
2013年8月1日 by admin
Adopt Standard: ASTM A387
Related grades we could supply:
ASTM A387 boiler and pressure vessel steel plate | ||
A387 Gr5 Cl2 is a chromium molybdenum alloy steel plates intended primarily for welded boiler and pressure vessels designed of elevated temperature service.
Our plates including A387 Gr5 Cl2 come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.
Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17
Steel dimension:
Thickness: 6MM to 300MM,
Width: 1500mm to 4050mm,
Length: 3000mm to 15000mm
A387 Grade 5 Cl2 steel Chemical requirement in Product analysis:
% | Mn % | P % | S % | SI % | Cr % | Mo % |
0.15 | 0.25-0.66 | 0.035 | 0.030 | 0.55 | 3.90-6.10 | 0.40-0.70 |
Ni % | V % | Nb % | B % | Nitrogen | | Tungsten |
| | | | | | |
Mechanical Property A387 Grade 5 Cl2:
Mechanical Property A387 Grade 5 Class 2 | A387 Grade 5 Class 2 |
Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in under [50mm], min, % | 515-690 310 …. 18 |
To find more about A387 Gr.5 Cl2 steel plate, or inquiry from our gangsteel, please feel free to CLICK HERE to contact us.
Tags: A387 Gr5 Cl.2 A387 Grade 5 Class 2 A387 Gr5 Cl2 ASTM A387 Gr.5 Cl.2