New Products /back


A514 Grade J,ASTM A514Gr.M ,A514 Grade J steel plate

2013年9月4日 by admin

Adopt Standard: ASTM A517

steel gradeA514 GRA,A514 GRB,A514 GRC,A514 GRE,A514 GRF,A514 GRH,A514 GRJ,A514 GRK,A514 GRM,A514 GRP,A514 GRQ,A514 GR R,A514 GRS,A514 GRT

 

A514 Grade J is for high yield strength, quenched and tempered alloy steel plate of structural quality in thickness of 50mm and under intended primarily for use in welded bridges and other structures.


The max thickness of A514 Grade J is 50mm. in the heat treatment, A514 Grade J shall be heat treatment by the mill to conform to the tensile and hardness requirements by heating to not less 900 degree and quenching in water or oil, tempering at not less 620 degree.

 

Gangsteel is the large agent in HBIS Wuyang mill and we have exported A514 Grade J to be used in oil platform project.

A514 Grade J steel Chemical requirement in Heat analysis

C  %

Mn  %

P  %

S %

SI %

Ni %

Cr %

0.12-0.21

0.45-0.70

0.035

0.035

0.20-0.35

1.20-1.50

 

Mo %

B %

V %

Ti %

Zr %

Cu %

Co %

0.45-0.60

0.001-0.005

 

 

 

 

 


Mechanical Property A514 Grade J

Mechanical Property A514 Grade J

A517 Grade J

20mm and under

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]

Elongation in under [50mm], min, %

Brinell Hardness Number

20mm-50mm

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in under [50mm], min, %

20mm and under

760-895

690

18

235-293

20mm-65mm

760-895

690

18


 

If you want to know price in A514 Grade J from Gangsteel, please inquiry us by email or calling to us, we will give our official quotation to you soon.

Tags: A514 GRA  A514 GRB  A514 GRC  A514 GRE  A514 GRF  A514 GRH  A514 GRJ  A514 GRK  A514 GRM  A514 GRP  A514 GRQ  A514 GR R  A514 GRS  A514 GRT  ASTM A514  A514 steel plate  steel plate  A514 Grade B supplier  A514 Grade E  A514 Grade Q  SA514 Gr. Q  SA514 GR A  SA514 GRB  SA514 Gr. E  SA514Gr. F  SA514 Gr. Q  

0 Comments, 0 Trackbacks