New Products /back


A515 Grade 60,A515 Gr 60,A515Gr.60,ASTM A515Gr60,steel plate

2011年4月14日 by admin

A515 Grade 60,A515 Gr 60,A515Gr60,A515 grade 60 steel,a516 gr 60 steel,a515gr.60 steel

 

Adopt Standard: A 515/A 515M-03
Gangsteel grade: A515 Grade 60,A515 Grade 65 and A515 Grade 70 steel grade.

 

A515 Grade 60 steel plate

A515/A515M specification covers carbon-silicon steel plates primarily for intermediate and higher temperature service in welded boilers and other pressure vessels projects.

 

A515 Grade 60 steel tensile strength is 415Mpa to 550Mpa and the yield strength is min 415Mpa.

 

About the thickness of A515 Gr 60, Gangsteel maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is 300mm. the delivery station is UT test, normalized and have to use the ingot to produce it.

A515 Grade 60 heat treatment, if a515 grade 60 steel thick in 50mm or under this thickness, A515 Grade 60 normalized supplied in the as-rolled condition. If our customer requirement, we also could do normalized. If A515 Grade 60 thicknesses above 50mm, this plate shall be normalized..

 

Our Gangsteel is specialized in super thick steel plate, and we also have much experience about A HIC test. We could provide DNV, ABS, LR ,BV,CCS,GL,CE mark certificate in our super thickness to promise our steel quality. We sincerely invite our new and old customer come to visit our mill for our long steel business.

 

 

A515 Grade 60 Chemical requirements

Carbon, max

%

Manganese, max

%

Silicon, max

%

25mm or under
25mm - 50mm
50mm- 100mm
100mm- 200mm
over 200mm

0.24
0.27
0.29
0.31
0.31

Heat Analysis

Product Analysis
      

0.90
0.98

Heat Analysis

Product Analysis

0.15-0.40

0.13-0.45

Phosphorus max

%

Sulfur max

%

 

 

All thickness

0.035

All thickness

0.035

 

 

             

 

 

A515 Grade 60 Tensile requirements

Mechanical Property

A515 Grade 60

Tensile strength, kis [MPa]

Yield strength, min, kis [MPa]
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

60-80 [415-550]
32 [220]

21

25

 

If any need in A515 Grade 60,a515gr60,a515 gr 60 steel plate, please feel free to contact our Gangsteel, we will give our competitive price, faster delivery and the best quality.

 

 

Tags: A515 Grade 60  A515 Gr 60  A515Gr60  A515 grade 60 steel  a516 gr 60 steel  a515gr.60 steel  

0 Comments, 0 Trackbacks