A515 Grade 65,A515 Gr 65,A515Gr65,A515 grade 65 steel plate
2011年4月14日 by admin
A515 Grade 65,A515 Gr 65,A515Gr65,A515 grade 65 steel,a516 gr 65 steel,a515gr.65 steel
Adopt Standard: A 515/A
Gangsteel grade: A515 Grade 60,A515 Grade 65 and A515 Grade 70 steel grade.
A515 Grade 65 steel plate
A515/A
A515 Grade 65 steel tensile strength is 450Mpa to 585Mpa and the yield strength is min 240Mpa.
About the thickness of A515 Gr 65, Gangsteel maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements.
Now, in our mill practice, Gangsteel normally limits the maximum thickness of plate is
A515 Grade 65 heat treatment, if a515 grade 65 steel thick in
Our Gangsteel is specialized in super thick steel plate, and we also have much experience about A HIC test. We could provide DNV, ABS, LR, BV, CCS, GL, CE mark certificate in our super thickness to promise our steel quality. We sincerely invite our new and old customer come to visit our mill for our long steel business.
A515 Grade 65 Chemical requirements
Carbon, max | % | Manganese, max | % | Silicon, max | % | |
| 0.28 | Heat Analysis Product Analysis | 0.90 | Heat Analysis Product Analysis | 0.15-0.40 0.13-0.45 | |
Phosphorus max | % | Sulfur max | % | | | |
All thickness | 0.035 | All thickness | 0.035 | | | |
A515 Grade 65 Tensile requirements
Mechanical Property | A515 Grade 65 |
Tensile strength, kis [MPa] Yield strength, min, kis [MPa] | 65-85 [450-585] 19 23 |
If any need in A515 Grade 65,a515gr65,a515 gr 65 steel plate, please feel free to contact our Gangsteel, we will give our competitive price, faster delivery and the best quality.
Tags: A515 Grade 65 A515 Gr 65 A515Gr65 A515 grade 65 steel a516 gr 65 steel a515gr.65 steel