New Products /back


A516GR55|A516Gr55 N|A516Gr55 HIC boiler steel plate

2013年8月19日 by admin

 ASTM A516 standard specification for pressure vessel plates, carbon steel for moderate and lower- temperature service.

ASTM A516 plates 40mm and under in thickness is normally supplied in the as-rolled condition. The plates may be ordered normalized or stress relieved, or both. ASTM A516 grade plates over 40mm in thickness shall be normalized.

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

Thickness: 6MM to 300MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm
 

Gangsteel is specialized in supplying ASTM A516 steel plate in A516 grade 55. For more information of A516 grade 55steel plates, please check them in following:

 

A516Gr55 Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

A516gr55

0.18-0.26

0.13-0.45

0.55-1.30

0.035

0.035

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Grade

 

A516 Grade 55 Mechanical Property

Thickness

Yield

Tensile

Elongation

A516gr55

mm

Min Mpa

Mpa

Min  %

6-50

205

380-515

27%

50-200

205

380-515

23%

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

 

Equivalent steel grade of A516 grade 55

Europe

Belgium

Germany

France

Italy

Sweden

India

Japan

 

 

E St E315

 

Fe 460-2-KG

SS29,12,01

 

 

 

If you need more stock steel plates in pressure vessel steel plate, please click warehouse sizes.

 

Related Grade: A516 Grade 60 | A516 Grade 65 |A516 grade 70

 

 

Tags: A516Gr55 HIC  A516GR55  A516Gr55 N  