New Products /back


A516Gr55|A516Gr55 N|A516Gr55 HIC steel plate

2013年8月12日 by admin

A516Gr55 Boiler and Pressure Vessel Steel Plate

 

Related Grade: A516 Grade60 | A516 Grade 65 | A516 Grade 55| A516 Grade 70

 

A516Gr55 steel is a carbon pressure vessel steel grade for moderate and lower temperature service for a variety of applications in the Petrochemical, Chemical, Oil & Gas Industries

 

A516Gr55 usual request normalized if thickness above 40mm, if not, Gangsteel usual delivery in hot rolled or control rolled station. A 516 Gr.55+N or A516gr55N mean that steel grade must be normalized in any thickness.

 

Gangsteel also supply the Ultrasonic test in thickness in A 435/A435M, A 577/577M and A 578/A578M to promise the perfect quality in long cooperation.

 

Our plates including A516 Gr55 come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

One of our boss is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

Dimension available to us:

Thickness: 6MM to 300MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm

 

A516Gr55 Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

A516gr55

0.18-0.26

0.13-0.45

0.55-1.30

0.035

0.035

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Grade

 

A516 Grade 55 Mechanical Property

Thickness

Yield

Tensile

Elongation

A516gr55

mm

Min Mpa

Mpa

Min  %

6-50

205

380-515

27%

50-200

205

380-515

23%

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

Equivalent steel grade of A516 grade 55

Europe

Belgium

Germany

France

Italy

Sweden

India

Japan

 

 

E St E315

 

Fe 460-2-KG

SS29,12,01

 

 

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about A516 Gr65 or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.  

Tags: A516GR55  A516Gr55 N  A516Gr55 HIC  A516 Grade 55  A516 Gr55 steel price  SA516 Gr55  A516 Gr55 steel plate  

None Comments, None Trackbacks