New Products /back


A516Gr65|A516Gr65 N|A516Gr65 HIC Boiler steel plate

2013年8月19日 by admin

A516Gr65 steel is a carbon pressure vessel steel grade for moderate and lower temperature service for a variety of applications in the Petrochemical, Chemical, Oil & Gas Industries

 

A516Gr65 usual request normalized if thickness above 40mm, if not, Gangsteel usual delivery in hot rolled or control rolled station. A 516 Gr.65+N or A516gr65N mean that steel grade must be normalized in any thickness.

 

Compare with the A 516Gr70, the A 516Gr65 steel grade have lower property in tensile and yield strength. Gangsteel also supply the Ultrasonic test in thickness in A 435/A435M, A 577/577M and A 578/A578M to promise the perfect quality in long cooperation.

 

Our plates including A516 Gr65 come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

A516Gr65 steel grade is a advantage Gangsteel company, we exported the super thickness steel plate max 140mm in A516Gr65 to Singapore in the best quality. One of our boss is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

The A 516 Grade 65 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

A516Gr65

0.24-0.29

0.13-0.45

0.79-1.3

0.035

0.035

 

The mechanical properties at A 516Gr65 steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

A516Gr70

6mm-40mm

240Mpa

450-585Mpa

23%

40mm-100mm

240Mpa

450-585Mpa

19%

The min impact energy is longitudinal energy

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about A516 Gr70 or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.  

Tags: A516Gr65  A516Gr65 hic  A516Gr65 n  