New Products /back


ASTM A516Gr.70,A516 Gr 70,A516 Grade 70 Steel plate

2011年4月14日 by admin

A516 Grade 70 Steel Grade

Steel Category: Boiler & pressure vessel steel plate

Adopt standard: A516 ASTM

Sell steel grade: A516 Grade 55 steel grade, A516 Grade 60 steel grade, A516 Grade 65 steel grade, A516 Grade 70 steel grade

 

A516 Grade 70 steel plate

 

A 516 Grade 70 steel is a carbon pressure vessel steel grade for moderate and lower temperature service.

 

A 516 Grade 70 usual request normalized if thickness above 40mm, if not , Gangsteel usual delivery in hot rolled or control rolled station. A 516 Gr.70+N or A516gr70N mean that steel grade must be normalized in any thickness.

 

Compare with the A 516 Grade 60, A 516 Grade 65, and A 516 Grade 55, the A 516 Grade 70 steel grade have better property in tensile and yield strength. Gangsteel also supply the Ultrasonic test in thickness in A 435/A435M, A 577/577M and A 578/A578M to promise the perfect quality in long cooperation.

 

A 516 Grade 70 steel grade is a advantage Gangsteel company, we exported the super thickness steel plate max 135mm in A 516 Gr.70 to Singapore in the best quality. One of our boss is the sales department manager of mill to promise the competitive price and the fastest delivery time to your projects.

 

If you have need in steel plate A 516 Grade 70, please check the stock list in A 516 Grade 70.

About A 516 Grade 70 detail informationplease check technical date in following.

 

 

The A 516 Grade 70 Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

A516 Gr 70

0.27-0.31

0.13-0.45

0.79-1.3

0.035

0.035

 

 

 

The mechanical properties at A 516 Grade 70 steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

A516 Gr.70

6mm-40mm

260Mpa

485-620Mpa

21%

40mm-100mm

260Mpa

485-620Mpa

17%

The min impact energy is longitudinal energy

 

 

 

If you have any need in A 516 Grade 70, please feel free to contact us soon by email or calling. We will reply to you as early as possible.

 

 

Tags: ASTM A516Gr.70  A516 Gr 70  A516 Grade 70 Steel plate  

0 Comments, 0 Trackbacks