ASTM A517 Grade A,A517 Grade A,A517 Grade A,steel plate
Adopt Standard: ASTM A517
Gang steel grade
ASTM A517 | A517 Grade A | A517 Grade B |
A517 Grade E | A517 Grade F | A517 Grade H |
A517 Grade P | A517 Grade Q | A517 Grade S |
A517 Grade A steel plate
A517 Grade A is a high strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure vessels.
A517 Grade A is a high strength quenched and tempered alloy steel plates intended for use in fusion welded boilers and other pressure vessels.
The maximum thickness of plate,
grade A and grade B are 32mm: Grade H and grade S are 50mm: grade P is 100mm: Grade F, is 65mm: Grade E and grade Q are 150mm in thickness
grade A and grade B are 32mm: Grade H and grade S are 50mm: grade P is 100mm: Grade F, is 65mm: Grade E and grade Q are 150mm in thickness
Gangsteel is a large agent in HBIS and cooperated with Wuyang Iron and steel co.,ltd to export high quality and super thickness steel plate. For the competitive price in A517 Grade A, please contact us by email.
A517 Grade A steel Chemical requirement in Product analysis
C % | Mn % | P % | S % | SI % | Ni % | Cr % |
0.13-0.23 | 0.74-1.20 | 0.035 | 0.035 | 0.34-0.86 | | 0.46-0.84 |
Mo % | B % | V % | Ti % | Zr % | Cu % | Co % |
0.15-0.31 | 0.025 | | | 0.04-0.16 | | |
Mechanical Property A517 Grade A
Mechanical Property A517 Grade A | A517 Grade A |
65mm and under Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in under [50mm], min, % 65mm-100mm Tensile strength, kis [MPa] Yield strength, min, kis [MPa] Elongation in under [50mm], min, % | 65mm and under 795-930 690 16 65mm-100mm 725-930 620 14 |