A572Gr50,A572 grade 50,A572 Gr 50,steel plate

2011年4月6日 by admin

Steel Category: Low alloy structural steel plate

Adopt standard: ASTM A 572/A 572M-06

 

A572 Grade 42 steel plate,A572 Grade 50 steel plate,A572 Grade 55 steel plate,A572 Grade 60 steel plate,A572 Grade 65 steel plate.

 

A 572 Grade 50 steel plates

 

A 572 Grade 50 steel plate is high strength low alloy columbium-vanadium structural steel grade. A 572 Grade 50 steel intended for riveted or bolted construction of bridges.

 

The equal steel grade is JIS SM570, GB Q460, EN S355JR and so on

 

Gangsteel has much experience in exporting A 572 Gr. 42, A 572 Gr.50, A572 Gr.55, A572 Gr.60 and A572 Gr.65. We cooperated with Korea and America Company in this steel grade and have a good reputation in steel quality.

 

If you have need in A572 Grade 50 steel plate, we will use our best quality and the fastest delivery time to satisfy your Demand.

 

For more information of A572 Grade 50, please refer them in following.

 

The Chemical is max composition of heat analysis:

 

Grade

C %

Si %

Mn %

P %

S %

V %

Ni %

Co %

A572 Gr.50

0.230

0.400

1.350

0.040

0.050

0.060

0.015

0.050

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield(Mpa)

Tensile(MPa)

Elongation(%)

A572 Grade 50

8mm-50mm

345Mpa

450Mpa

21%

50mm-200mm

345Mpa

450Mpa

18%

The min impact energy is longitudinal energy

 

 

If you want to purchase more yield and tensile steel grade, please check steel grade in A572 Grade 55, A572 Grade 60, A572 Grade 70 steel grade.

 

 

If you need our A572 Grade 50 steel grade in stock, please click .Gangsteel Stock.List to find stock steel grade.

 

For more information in quality certificate or inquiry in competitive official quotation, please contact us by email.

 

 

Tags: A572Gr50  A572 grade 50  A572Gr.50  

0 Comments, 0 Trackbacks