A588 Grade B steel plate

 

A588 Grade B steel plate is for high strength low alloy structural steel with 345Mpa minimum yield point to 100mm thickness.

 

When propertly exposed to the atmosphere, A588 Grade B is suitable for many applications in the bare condition. A588 Grade B could be produced in 200mm in our Gangsteel mill.

 

Gangsteel has much experience for exporting A588 Grade B and also supply our customers in supplementary requirement in S2, S3, S5, S6, S8, S15, S18, S30 and so on.

 

If you could need the equal steel grade with A588 Grade, you could choose the 09CuPCrNi-A, 09CuPCrNi-B,05CuPCrNi,S355J0WP,S355J2WP,Corten A, Corten B Grade steel.

 

A588 Grade B steel Chemical composition in Product analysis

 

Carbon, %

 

Manganese, %

Cr %

Silicon %

N % max

Sulfur %

 

Max  0..20

 

0.75-1.35

0.40-0.70

0.15-0.5

0.010

0.05

 

Cu  %

 

Phosphorus %

Ni %

Mo %

 

 

 

0.20-0.40

 

0.04

0.5

….

 

 

 

A588 Grade B steel Mechanical Properties

Mechanical Property of A588GrB steel plate

A588 Grade B,A588Gr B

Tensile strength, kis [MPa]

100mm or under

100mm-125mm
125mm-200mm

Yield strength, min, kis [MPa]

100mm or under

100mm-125mm
125mm-200mm

Elongation in under [50mm], min, %

Elongation in under [50mm-200mm], min, %

Tensile strength, kis [MPa]

[485]

[460]

[435]

Yield strength, min, kis [MPa]

[345]

[315]

[290]

21

18

 

 

Gangsteel also could supply the stock steel grade in A588 Grade B, Any need in A588 Grade B steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.

 

A588GrB,A588 Grade B,A588GrB steel,A588 Gr B grade,A588 Grade B steel,A588Gr.B

 

 

Tags: A588GrB  A588 Grade B  A588GrB steel  A588 Gr B grade  A588 Grade B steel  A588Gr.B  

0 Comments, 0 Trackbacks