Adopt Standard: A588/A588M-01
Gangsteel steel grade: A588 Grade A,A588 Grade B,A588 Grade C,A588 Grade K,A588GrA, A588GrB,A588GrC,A588GrK steel grade.

 

A588 Grade C steel plate

 

A588 Grade C usual be used in welded bridges and building where savings in weight or added durability are important.

 

A588 Grade C, the atmospheric corrosion resistance of this steel in most environments is substantially better than that of carbon structural steels with or without copper addition.

 

Gangsteel has much experience for exporting A588 Grade C and also supply our customers in supplementary requirement in S2, S3, S5, S6, S8, S15, S18, S30 and so on.

 

If you could need the equal steel grade with A588 Grade, you could choose the 09CuPCrNi-A, 09CuPCrNi-B,05CuPCrNi,S355J0WP,S355J2WP,Corten A, Corten B Grade steel.

 

A588 Grade C steel Chemical composition in Product analysis

 

Carbon, %

 

Manganese, %

Cr %

Silicon %

N % max

Sulfur %

Max  0.15

 

0.80-1.35

0.30-0.50

0.15-0.40

0.010

0.05

Cu  %

 

Phosphorus %

Ni %

Mo %

Vanadium

 

0.20-0.50

 

0.04

0.20-0.50

….

0.02-0.10

 

A588 Grade C steel Mechanical Properties

Mechanical Property of A588Gr C steel plate

A588 Grade C,A588Gr C

Tensile strength, kis [MPa]

100mm or under

100mm-125mm
125mm-200mm

Yield strength, min, kis [MPa]

100mm or under

100mm-125mm
125mm-200mm

Elongation in under [50mm], min, %

Elongation in under [50mm-200mm], min, %

Tensile strength, kis [MPa]

[485]

[460]

[435]

Yield strength, min, kis [MPa]

[345]

[315]

[290]

21

18

 

 

Gangsteel also could supply the stock steel grade in A588 Grade C, Any need in A588 Grade C steel grade, please feel free to contact us by email or calling to us, we will reply our competitive price to you soon.

 