A588 GRA,A588 GRB,A588 GRC,A588 GRK weather resistant steel plate

 

A588 steel plate is for high strength low alloy structural steel.

 

1. Steel Grade: A588 Grade A, A588 Grade B, A588 Grade C, A588 Grade K, Corten A, Corten B

2. Steel Dimension: Thickness: 6-200mm, Width: 1500-4050mm, Length: 3000-15000mm

3. Adopt Standard: ASTM A588

4. Delivery Condition: Hot rolled, CR, Normalized, Quenched, Tempering, TMCP.

5. Delivery Time: 30days

6. Payment Item: L/C, TT

7. Trade Terms: FOB, CFR or CIF

8. Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, and so on.

9. Certificate: ABS, DNV, BV, LR, GL, CSS, KR, NK,RINA, TUV, CE, ISO, and so on.

 

Henan Gang Iron and Steel Co. Ltd (Gangsteel) is specialized in supplying weather resistant steel plates. We have ten years experience in the exportation of steel plates in EN 10025-5, ASTM A588, Corten A, Corten B, EN 10155, JIS3114, BS4360, ISO 4952, GB 4172, GB4171, NFA 35502, and so on. The thickness we could supply can be up to 300mm.

  

Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company. We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.

 

Yours sincerely,

Ms. Olina

 

 

Henan Gang Iron and Steel Co., Ltd

Cell: 86-15226033579

Tel: 86-0371-55830820  Fax: 86-0371-88884766
Email: olina@gangsteel.com
Skype: gangsteel18
MSN: gangsteel18@hotmail.com

Gmail: gangsteel18@gmail.com

 

Tags: A588 Grade A  A588 Grade B  A588 Grade C  A588 Grade K  A588 Gr.A  A588 Gr.B  A588 Gr.C  A588 Gr.K  A588 GRA  A588 GRB  A588 GRC  A588 GRK  ASTM A588 Gr. A  ASTM A588 Gr. B  ASTM A588 Gr. C  A588 Gr. K  ASTM A588  A588 Gr. A supplier  ASTM A588 weathering steel plate  

0 Comments, 0 Trackbacks