BV A500 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.
For more information in BV A500 steel grade, please refer to the following:
BV A500 Chemical composition heat analysis
Element | BV A500 Max % | Element | BV A500 max % |
C | 0.21 | Ni | 2.0 |
Mn | 1.70 | Mo | 1.0 |
Si | 0.10-0.55 | Al | 0.015 min |
S | 0.035 | Nb | 0.06 |
P | 0.035 | V | 0.10 |
Cu | 1.5 | Ti | 0.20 |
Cr | 2.0 | N | 0.020 |
BV A500 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | 0 degree | |
BV A500 | 8-260 | 500 | 610-770 | 16 | 33J |
Note: the impact energy under less 150mm thickness