BV A690 Steel Plate

 
BV A690 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV A690 steel grade, please refer to the following:

 
 
 
 
BV A690 Chemical composition heat analysis

Element
BV A690 Max %
Element
BV A690 max %
C
0.21
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
   Al
 0.015 min
S
0.035
   Nb
0.06
P
0.035
V
0.10
Cu
1.5
Ti
0.20
    Cr
2.0
N
0.020

           
 
 
 
 
BV A690 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
BV A690
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 
 