BV/AH36,BV AH36,AH36,AH36 steel,BV/AH36 steel,BV AH36,steel,BV Steel plate
2011年3月9日 by admin
BV/AH36,BV AH36,AH36,AH36 steel,BV/AH36 steel,BV AH36,steel,BV Steel plate
Henan Gang iron and steel co., Ltd supply steel grade BV/A, BV/B, BV/D, BV/E, BV/AH36, BV/DH36, BV/EH36, BV/FH36, BV/AH32, BV/DH32, BV/EH32, BV/FH32
In usual if AH36 steel plate thickness above 50mm, mill request the normalized in hot rolled plate Or control rolled, if above 150mm thickness our mill also could use the electroslag remelting technical in ingot to do for our customers.
AH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:
Thickness: 6mm to 300mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 300mm which beyond nine classification society approval.
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly in our mill cost price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
We sincerely hope old and new customers to visit our mill for a long steel business
About AH36 detail information,please refer to technical date in following.
The Chemical is max composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
AH36 | 0.180 | 0.1-0.5 | 0.90-1.6 | 0.035 | 0.035 | 0.05-0.10 | 0.015 | 0.200 |
Cu % | Mo % | Nb % | Ni % | Ti % | | | | |
0.350 | 0.080 | 0.02-0.05 | 0.400 | 0.020 | | | |
The mechanical properties at ambient temperature for quenched and tempered steel plate
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
AH36 | 8mm-50mm | Min 355Mpa | 490-620Mpa | 21% | 0 | 34J |
51mm-70mm | Min 355Mpa | 490-620Mpa | 21% | 0 | 41J | |
71mm-100mm | Min 355Mpa | 490-620Mpa | 21% | 0 | 50J | |
The min impact energy is longitudinal energy |
If you have any need ABS AH36 steel plate, please feel free to contact us soon.
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
0 Comments, 0 Trackbacks