BV D420 | BV D420 STEEL PLATE
2011年10月26日 by admin
BV D420 STEEL PLATE
BV D420 steel grade shall be killed and find grain treated. Steel grade of strength levels up to and including 500Mpa should be supplied in Normalized, TM or QT condition. Steel grade of strength levels above 500Mpa shall be supplied in TM or QT delivery condition.
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.
For more information in BV D420 steel grade, please refer to the following:
BV D420 Chemical composition heat analysis
Element | BV D420 Max % | Element | BV D420 max % |
C | 0.20 | Ni | 2.0 |
Mn | 1.70 | Mo | 1.0 |
Si | 0.10-0.55 | Al | 0.015 min |
S | 0.030 | Nb | 0.06 |
P | 0.030 | V | 0.10 |
Cu | 1.5 | Ti | 0.20 |
Cr | 2.0 | N | 0.020 |
BV D420 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -20 degree | |
BV D420 | 8-260 | 420 | 530-680 | 18 | 28J |
Note: the impact energy under less 150mm thickness
Related Grade: NV D420 | BV D460