BV D460 | BV D460 STEEL PLATE
2011年10月26日 by admin
BV D460 STEEL PLATE
BV D460 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting Extra high strength steel grade.
For more information in BV D460 steel grade, please refer to the following:
BV D460 Chemical composition heat analysis
Element | BV D460 Max % | Element | BV D460 max % |
C | 0.20 | Ni | 2.0 |
Mn | 1.70 | Mo | 1.0 |
Si | 0.10-0.55 | Al | 0.015 min |
S | 0.030 | Nb | 0.06 |
P | 0.030 | V | 0.10 |
Cu | 1.5 | Ti | 0.20 |
Cr | 2.0 | N | 0.020 |
BV D460 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -20 degree | |
BV D460 | 8-260 | 460 | 570-720 | 17 | 31J |
Note: the impact energy under less 150mm thickness
Related Grade: NV D460 | BV D500