BV D500 Chemical composition heat analysis
Element | BV D550 Max % | Element | BV D550 max % |
C | 0.20 | Ni | 2.0 |
Mn | 1.70 | Mo | 1.0 |
Si | 0.10-0.55 | Al | 0.015 min |
S | 0.030 | Nb | 0.06 |
P | 0.030 | V | 0.10 |
Cu | 1.5 | Ti | 0.20 |
Cr | 2.0 | N | 0.020 |
BV D500 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -20 degree | |
BV D500 | 8-260 | 500 | 610-770 | 16 | 33J |
Note: the impact energy under less 150mm thickness