For more information in BV D620 steel grade, please refer to the following:

 
 
BV D620 Chemical composition heat analysis

Element
BV D620 Max %
Element
BV D620  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
BV D620 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
BV D620
8-260
620
720-890
15
41J

Note: the impact energy under less 150mm thickness
 
 
 