New Products /back


BV EH40 steel grade, BV Grade,BV EH40,EH40

2011年3月27日 by admin

BV EH40 steel grade, BV Grade

BV steel grade:

BV/A

BV/B

BV/D

BV/E

BV/AH36

BV/DH36

BV/EH36

BV/FH36

BV/AH32

BV/DH32

BV/EH32

BV/FH32

BV/AH40

BV/DH40

BV/EH40

BV/FH40

LR

DNV

ABS

GL

 

Adopt Standard: BV classification society

BV EH40 steel grade

 

Our mill could produce size in the following:
Thickness: 6mm to 220mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, GL EH32 Z15, GL EH32 Z25, GL EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

BV grade thickness tolerance should be in +-0.3mm.

 

Henan Gang iron and steel co., Ltd is specialized at super thick steel plate which beyond nine classification society approval in thickness. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers.

 

Gangsteel exported BV EH40 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About BV EH40 detail information, please refer to technical date in following.

 

BV EH40 Chemical composition heat analysis

Element

BV EH40 Max %

Element

BV EH40 max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

0.0015 min

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.05-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

BV EH40 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

BV EH40

8-220

390

510-650

20

41J

Note: the impact energy under less 50mm thickness

 

If you have any need in BV EH40 steel plate, please feel free to contact us soon to get a competitive price.

 

Tags: BV EH40  BV Grade EH40  EH40  

0 Comments, 0 Trackbacks