BV FH32,FH32,BV Grade FH32
2011年3月27日 by admin
BV FH32 Steel grade, BV Grade
BV steel grade:
BV/A | BV/B | BV/D | BV/E |
BV/AH36 | BV/DH36 | BV/EH36 | BV/FH36 |
BV/AH32 | BV/DH32 | BV/EH32 | BV/FH32 |
BV/AH40 | BV/DH40 | BV/EH40 | BV/FH40 |
LR | DNV | ABS | GL |
Adopt Standard: BV classification society
BV FH32 steel grade
Our mill could produce size in the following:
Thickness: 6mm to 220mm,
Width: 1500mm to 4020mm
Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, GL EH32 Z15, GL EH32 Z25, GL EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.
BV grade thickness tolerance should be in +-0.3mm.
Gangsteel exported BV FH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.
We sincerely hope old and new customers to visit our mill for a long steel business
About BV FH32 detail information, please refer to technical date in following.
BV FH32 Chemical composition heat analysis
Element | BV FH32 Max % | Element | BV FH32 max % |
C | 0.16 | Ni | 0.40 |
Mn | 0.90-1.60 | Mo | 0.08 |
Si | 0.50 | Al | 0.0015 min |
S | 0.025 | Nb | 0.20-0.05 |
P | 0.025 | V | 0.05-0.10 |
Cu | 0.35 | Ti | 0.02 |
Cr | 0.20 | N | 0.009 |
BV FH32 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -60 degree | |
BV DH36 | 8-220 | 315 | 490-620 | 22 | 31J |
Note: the impact energy under less 50mm thickness
If you have any need in BV FH32 steel plate, please feel free to contact us soon to get a competitive price.
Tags: BV FH32 Grade FH32 FH32 steel plate
0 Comments, 0 Trackbacks