BV FH36 Steel grade, BV Grade

BV steel grade:

BV/A

BV/B

BV/D

BV/E

BV/AH36

BV/DH36

BV/EH36

BV/FH36

BV/AH32

BV/DH32

BV/EH32

BV/FH32

BV/AH40

BV/DH40

BV/EH40

BV/FH40

LR

DNV

ABS

GL

 

Adopt Standard: BV classification society

BV FH36 steel grade

 

Our mill could produce size in the following:
Thickness: 6mm to 220mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, GL EH32 Z15, GL EH32 Z25, GL EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

BV grade thickness tolerance should be in +-0.3mm.

 

Henan Gang iron and steel co., Ltd is specialized at super thick steel plate which beyond nine classification society approval in thickness. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers.

 

Gangsteel exported BV FH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About BV FH36 detail information, please refer to technical date in following.

 

BV FH36 Chemical composition heat analysis

Element

BV FH36 Max %

Element

BV FH36 max %

C

0.16

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

0.0015 min

S

0.025

   Nb

0.20-0.05

P

0.025

V

0.05-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

0.009

           

BV FH36 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-60 degree

BV DH36

8-220

355

490-620

21

34J

Note: the impact energy under less 50mm thickness

 

If you have any need in BV FH36 steel plate, please feel free to contact us soon to get a competitive price.

 

 