BV E420 extra high grade steel plate
 
Adopt standard: BV Extra high strength steel plate
BV Extra High Grade:
 
BV E420 steel grade.
 
BV E420 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
BV E420 steel grade shall be killed and find grain treated. Steel grade of strength levels up to and including 500Mpa should be supplied in Normalized, TM or QT condition. Steel grade of strength levels above 500Mpa shall be supplied in TM or QT delivery condition.
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV E420 steel grade, please refer to the following:

 
BV E420 Chemical composition heat analysis

Element
BV E420 Max %
Element
BV E420  max %
C
0.20
Ni
0.40
Mn
1.70
Mo
0.08
Si
 0.10-0.55
   Al
 0.020 min
S
0.030
   Nb
0.20-0.05
P
0.030
V
0.05-0.10
Cu
0.35
Ti
0.0007-0.05
    Cr
0.20
N
 

            
BV E420 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E420
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
If you have any need in BV E420 steel plate, please feel free to contact us soon to get a competitive price.
 
BV E420,BV E420,E420 steel grade, BV Grade E420, E420 steel plate
 

Tags: BV E420  extra high grade steel plate  

0 Comments, 0 Trackbacks