New Products /back


Corten B,Cor-Ten B,Corten B steel,Corten B steel plate

2011年4月14日 by admin

Corten B,Cor-Ten B,Corten B steel,Corten B grade,Corten B steel plate,Corten B plate.

Adopt Standard: Corten b,Cor-Ten B
Gangsteel sell grade: Corten A, Corten B, Cor-Ten A,Cor-Ten B,steel plate

Corten b steel plate

 

Corten B or Cor-Ten B is a weather resistant steel and the chemical composition of Corten b OR Cor-Ten B has been designed to provide a high resistance to atmospheric corrosion, especial in urban environment. Corten b or Cor-Ten b is a copper chromium alloy steel – this alloy displays a greater level of resistance to atmospheric weathering when compared to other unalloyed steels.


The protective layer of Corten b constantly develops and regenerates over time, reacting to the pollutants in the atmosphere. Consideration should be made with regard to the thicknesses used especially when the material is utilized for structural rather than solely cosmetic purposes. 

Gangsteel exported Corten B steel plate many years and our mill has much experience in Corten B steel grade. The different item is the element of P between Corten B and the Corten A steel grade.

Gangsteel supply Corten B in normalized station in ingot steel, the normalized temperature is 910dgree+-10 degree and total heating time have to above 1.5min/mm. The Furnace temperature should be 920-+10 degree, heating insulation time should be above 1.5min/mm.

Corten B or Cor-Ten B steel plate Chemical Requirement

Carbon, %

V %

Manganese, %

Cr %

Silicon, %

 

Sulfur %

 

0.19

0.02-0.10

0.7-0.80

0.40-0.65

0.30-0.65

 

0.030

 

Cu  %

 

Phosphorus %

 

Nickel %

 

AL %

 

0.25-0.40

 

0..035

 

0.40

 

0.020-0.06

 

 

 

Corten B steel Tensile Requirements

 

Mechanical Property of Corten B steel plate

Corten B  Equal S355J2W

Tensile strength, kis [MPa]

50mm or under

Yield strength, min, kis [MPa]

50mm or under
Elongation in under [50 mm], min, %

Tensile strength, kis [MPa]

[485-490]

Yield strength, min, kis [MPa] [345]

20

 

Gangsteel sincerely invite our customer to visit our mill and inquiry Corten B steel grade from gangsteel, we will give our faster delivery and more competitive price for our long cooperation.

Corten B,Cor-Ten B,Corten B steel,Corten B grade,Corten B steel plate,Corten B plate.

 

Tags: Corten B  Cor-Ten B  Corten B steel  Corten B grade  Corten B steel plate  Corten B plate  

0 Comments, 0 Trackbacks