New Products /back


DNV DH27S,NV D27S,DNV Grade DH27S,DNV Grade

2011年3月28日 by admin

DNV Grade, DNV DH27S,NV D27S,DNV Grade DH27S

 

Adopt Standard: DNV

DNV steel grade:

NV E

NV D

NV A

NV B

NV A32

NV D32

NV E32

NV F32

NV A40

NV D40

NV E40

NV F40

NV A36

NV D36

NV E36

NV F36

LR

ABS

GL

BV

 

DNV DH27S steel grade

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, GL EH32 Z15, GL EH32 Z25, GL EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

 

Henan Gang iron and steel co., Ltd is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers.

 

Gangsteel exported DNV DH27S steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About DNV DH27S detail information, please refer to technical date in following.

 

DNV DH27S Chemical composition heat analysis

Element

DNV DH27S Max %

Element

DNV DH27S max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.10-0.50

   Al

0.020-0.085

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.05-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

 

DNV DH27S Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

DNV DH27S

8-240

265

400-530

22

27J

Note: the impact energy under less 50mm thickness

 

If you have any need in DNV DH27S steel plate, please feel free to contact us soon to get a competitive price.

 

 

Tags: DNV DH27S  NV D27S  DNV Grade DH27S  