NV D36,DNV DH36,DH36,DH36 steel,NV D36 steel,DNV DH36,DNV DH40
2011年3月9日 by admin
NV D36,DNV DH36,DH36,DH36 steel,NV D36 steel,DNV DH36,DNV DH40
Henan Gang iron and steel co., Ltd supply steel grade DNV Grade A, DNV Grade B, DNV Grade D, DNV Grade E, DNV AH32, DNV DH32, DNV EH32, DNV FH32, DNV AH36, DNV DH36, DNV EH36, DNV FH36, NV A36, NV E36, NV F36, NV A32, NV D32, NV E32, NV F32, NV D, NV E, NV A , NV B steel grade.
ABS DH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:
Thickness: 6mm to 180mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
Henan Gang iron and steel co., Ltd also could supply super thickness plate which beyond nine classification society approval.
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for long steel business
About DH36 detail information,please refer to technical date in following.
The Chemical is max composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
DH36 | 0.180 | 0.1-0.5 | 0.90-1.6 | 0.035 | 0.035 | 0.05-0.10 | 0.015 | 0.200 |
Cu % | Mo % | Nb % | Ni % | Ti % | | | | |
0.350 | 0.080 | 0.02-0.05 | 0.400 | 0.020 | | | |
The mechanical properties at ambient temperature for quenched and tempered steel plate
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
DH36 | 8mm-50mm | Min 355Mpa | 490-620Mpa | 21% | -20 | 34J |
51mm-70mm | Min 355Mpa | 490-620Mpa | 21% | -20 | 41J | |
71mm-100mm | Min 355Mpa | 490-620Mpa | 21% | -20 | 50J | |
The min impact energy is longitudinal energy |
Our mill DH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in DH36 steel plate, please feel free to contact us soon.