New Products /back


NV E32,EH32,DNV EH32,EH32 steel,NVE32 steel,DNV EH32,steel plate,EH32

2011年3月9日 by admin

 

NV E32,EH32,DNV EH32,EH32 steel,NVE32 steel,DNV EH32,steel plate,EH32
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade DNV Grade A, DNV Grade B, DNV Grade D, DNV Grade E, DNV AH32, DNV DH32, DNV EH32, DNV FH32, DNV AH36, DNV DH36, DNV EH36, DNV FH36, NV A36, NV E36, NV F36, NV A32, NV D32, NV E32, NV F32, NV D, NV E, NV A , NV B steel grade.
 
 
 
In EH32 steel plate, our mill have more ingot to provide super thick steel plate, our max per weight of plate is above 24.5mt now, max width is 4000mm..
 
EH32 steel grade is lower than FH32 in yield and tensile strength. It is a good material for shipbuilding in deck. EH32 Grade is in -40 impact test of 34J energy. All of thickness of EH32 material need normalize in delivery station.
 
Henan Gang iron and steel co., Ltd supply EH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for a long steel business.
 
About EH32 detail information,please check technical date in following.
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 EH32
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
EH32
8mm-50mm
Min 315Mpa
440-590Mpa
22%
-40
 34J
51mm-70mm
Min 315Mpa
440-590Mpa
22%
-40
 38J
71mm-100mm
Min 315Mpa
440-590Mpa
22%
-40
 46J
The min impact energy is longitudinal energy

 
 
Our mill EH32 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in EH32 steel plate, please feel free to contact us soon.
 
 

Tags: NV E32  EH32  DNV EH32  EH32 steel  NVE32 steel  DNV EH32  steel plate  EH32  