DNV EH32 STEEL PLATE

2012年2月28日 by admin

                                    DNV EH32 STEEL PLATE

 

 

Gangsteel is specialized in supplying DNV high strength steel plate in DNV Grade E32. For more information of Grade E32 steel plate, please check them in following:

 

DNV EH32 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

DNV EH32

0.18

0.10-0.50

0.9-1.6

0.035

0.035

0.015-0.08

-

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.40

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

 

 

DNV EH32 high general strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

DNV EH32

mm

Min Mpa

Mpa

Min  %

-40

J

J

t≤50

315

440-590

22%

22

31

50t≤70

315

440-590

22%

26

38

70t≤150

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

 

Equivalent steel grade of DNV EH32

ABS

GL

LR

BV

CCS

NK

KR

RINA

AB/EH32

GL-E32

LR/EH32

BV/EH32

CCS/E32

K E32

R E32

RI/E32

 

 

 

 

 

 

Tags: DNV EH32  DNV Grade EH32  

0 Comments, 0 Trackbacks