DNV A460 shipbuilding and offshore platform steel plate

2013年8月1日 by admin

Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV Grade A460. For more information of Grade A460 steel plate, please check them in following:

 

DNV Steel Plate Grade

General Strength

NV A

NV B

NV D

NV E

High Strength

NV A32

NV D32

NV E32

NV F32

NV A36

NV D36

NV E36

NV F36

NV A40

NV D40

NV E40

NV F40

Extra Strength

NV A420

NV D420

NV E420

NV F420

NV A460

NV D460

NV E460

NV F460

NV A500

NV D500

NV E500

NV F500

NV A550

NV D550

NV E550

NV F550

NV A620

NV D620

NV E620

NV F620

NV A690

NV D690

NV E690

NV F690

 

NV A460 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV A550

0.21

0.10-0.55

1.7

0.035

0.035

0.015-0.08

0.020

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.04-0.10

0.02

 

 

0.005

 

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

NV A460 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV A550

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

460

570-720

17%

31

46

50t≤70

460

570-720

17%

31

46

70t≤150

460

570-720

17%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV A460

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/AQ46

R A46

LR/AH46

BV/A460

CCS/A460

K A46

GL-A460

RI/A460

To find more about shipbuilding steel plate, or inquiry from our gangsteel, please feel free to CLICK HERE to contact us.

Tags: DNV A460  NV A460  NV A460 steel plate  DNV Grade A460  AB/A460  