DNV AH32 STEEL PLATE

2012年2月28日 by admin

DNV AH32 STEEL PLATE

 

 Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV AH32 For more information of DNV AH32 steel plate, please check them in following:

 

DNV AH32 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV/AH32

0.18

0.10-0.50

0.9-1.6

0.035

0.035

0.015-0.08

 

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.40

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

DNV AH32 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV/AH32

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

315

440-590

22%

22

31

50t≤70

315

440-590

22%

26

38

70t≤150

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV/AH32

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/AH32

R AH32

LR/AH32

BV/AH32

CCS/AH32

K AH32

GL-AH32

RI/AH32

 

 If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 

 

Tags: DNV Grade EH32  NV E32  DNV EH32  NV E32 steel grade  NV-E32  DNV steel  DNV EH32 steel plate  

0 Comments, 0 Trackbacks