New Products /back


DNV AH36 STEEL PLATE

2012年2月28日 by admin

DNV AH36 STEEL PLATE

 

 Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV AH36 For more information of DNV AH36 steel plate, please check them in following:

 

DNV AH36 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV/AH36

0.18

0.10-0.50

0.9-1.6

0.035

0.035

0.015-0.08

 

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.40

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

DNV AH36 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV/AH36

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

355

490-620

21%

24

34

50t≤70

355

490-620

21%

27

41

70t≤150

355

490-620

21%

34

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV/AH36

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/AH36

R AH36

LR/AH36

BV/AH36

CCS/AH36

K AH36

GL-AH36

RI/AH36

 

 If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 

 

Tags: DNV Grade AH36  NV A36  DNV AH36  NV A36 steel grade  NV-A36  DNV steel  DNV AH36 steel plate  DNV AH36 MARINE STEEL  