DNV FH40 STEEL PLATE

 

 Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV FH40. For more information of DNV FH40 steel plate, please check them in following:

 

DNV FH40 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV/FH40

0.16

0.10-0.50

0.9-1.6

0.025

0.025

0.015-0.08

 

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.80

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

DNV FH40 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV/FH40

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

390

510-650

20%

27

41

50t≤70

390

510-650

20%

30

45

70t≤150

390

510-650

20%

37

55

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV/FH40

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/FH40

R FH40

LR/FH40

BV/FH40

CCS/FH40

K FH40

GL-FH40

RI/FH40

 

 If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 

 

Tags: DNV Grade FH40  NV F40  DNV FH40  NV F40 steel grade  NV-F40  DNV marine steel  

0 Comments, 0 Trackbacks