DNV GRADE E STEEL PLATE

 

 Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV Grade E. For more information of Grade E steel plate, please check them in following:

 

NV/E extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV/E

0.18

0.10-0.35

0.70

0.035

0.035

0.015

 

Nb

V

Ti

Cu

B

Ni

Mo

 

 

 

 

 

 

 

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

NV/E extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV/E

mm

Min Mpa

Mpa

Min  %

-40

J

J

t≤50

235

400-520

22%

20

27

50t≤70

235

400-520

22%

24

34

70t≤150

235

400-520

22%

27

41

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of NV/E

ABS

KR

LR

BV

CCS

NK

GL

RINA

AB/E

R E

LR/E

BV/E

CCS/E

K E

GL-E

RI/E

 

 If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 

 

Tags: DNV GRAD E  NV E  NV/E  NV E steel plate  DNV steel grade  

0 Comments, 0 Trackbacks