DNV E620,NV E620,E620 steel grade, DNV Grade E620,E620 steel plate
2011年3月28日 by admin
DNV E620,NV E620,E620 steel grade, DNV Grade E620,E620 steel plate
Adopt standard: DNV Extra high strength steel plate
DNV Extra High Grade:
NV A420 | NV D420 | NV E420 | NV F420 |
NV A460 | NV A500 | NV A550 | NV E420 |
NV F420 | NV D460 | NV E460 | NV F460 |
NV D500 | NV E500 | NV F500 | NV D550 |
NV E550 | NV F550 | NV D620 | NV D690 |
NV E690 | NV F690 | NV A620 | NV A690 |
NV E620 steel grade.
NV E620 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in NV A690.
NV E620 steel grade shall be killed and find grain treated. Steel grade of strength levels up to and including 500Mpa should be supplied in Normalized, TM or QT condition. Steel grade of strength levels above 500Mpa shall be supplied in TM or QT delivery condition.
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.
For more information in NV E620 steel grade, please refer to the following:
NV E620 Chemical composition heat analysis
Element | NV E620 Max % | Element | NV E620 max % |
C | 0.20 | Ni | 0.40 |
Mn | 1.70 | Mo | 0.08 |
Si | 0.10-0.55 | Al | 0.020 min |
S | 0.030 | Nb | 0.20-0.05 |
P | 0.030 | V | 0.05-0.10 |
Cu | 0.35 | Ti | 0.0007-0.05 |
Cr | 0.20 | N | |
NV E620 Mechanical properties, longitudinal min impact energy
Grade | Thickness | Yield Strength | Tensile Strength | Elongation | Impact Energy |
(mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| | | | -40 degree | |
NV E620 | 8-260 | 620 | 720-890 | 15 | 41J |
Note: the impact energy under less 150mm thickness
If you have any need in NV E620 steel plate, please feel free to contact us soon to get a competitive price.
DNV E620,NV E620,E620 steel grade, DNV Grade E620, E620 steel plate
Tags: DNV E620 NV E620 DNV Grade E620
0 Comments, 0 Trackbacks