NV A500 shipbuilding steel plate
2013年8月1日 by admin
Gangsteel is specialized in supplying DNV extra high strength steel plate in DNV Grade A550. For more information of Grade A550 steel plate, please check them in following:
NV A550 extra high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
NV A550 | 0.21 | 0.10-0.55 | 1.7 | 0.035 | 0.035 | 0.015-0.08 | 0.020 |
Nb | V | Ti | Cu | B | Ni | Mo | |
0.02-0.05 | 0.04-0.10 | 0.02 | | | 0.005 | |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
NV A550 extra high general strength property | |||||||
Grade | | | Mechanical Property | | |||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
NV A550 | mm | Min Mpa | Mpa | Min % | 0 | J | J |
t≤50 | 550 | 670-830 | 16% | 37 | 55 | ||
50<t≤70 | 550 | 670-830 | 16% | 37 | 55 | ||
70<t≤150 | 550 | 670-830 | 16% | 37 | 55 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
Equivalent steel grade of NV A550 | |||||||
KR | LR | BV | CCS | NK | GL | RINA | |
AB/AQ56 | R A56 | LR/AH55 | BV/A550 | CCS/A550 | K A56 | GL-A550 | RI/A550 |