New Products /back


NV F620|DNV F620 steel plate

2013年8月8日 by admin

Gangsteel is specialized in supplying extra high strength steel plate in Grade F620 approved by DNV, ABS, RINA, LR, GL, BV, CCS, NK and KR.

 

For more information of DNV Grade F620 steel plate, please check them in following:

 

DNV Steel Plate Grade

General Strength

NV A

NV B

NV D

NV E

High Strength

NV A32

NV D32

NV E32

NV F32

NV A36

NV D36

NV E36

NV F36

NV A40

NV D40

NV E40

NV F40

Extra Strength

NV A420

NV D420

NV E420

NV F420

NV A460

NV D460

NV E460

NV F460

NV A500

NV D500

NV E500

NV F500

NV A550

NV D550

NV E550

NV F550

NV A620

NV D620

NV E620

NV F620

NV A690

NV D690

NV E690

NV F690

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.


Steel Services: Cutting, Painting, Pretreatment, Ultrasonic Test, Third Party Inspection, and so on.

 

Gangsteel exported DNV F620 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

  

DNV GRADE F620 Chemical composition heat analysis:

NV F620 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV F620

0.18

0.10-0.55

1.6

0.025

0.025

0.015-0.08

0.020

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.04-0.10

0.02

 

0.005

 

 

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

 

NV F620 extra high general strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV F620

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

620

720-890

15%

41

62

50t≤70

620

720-890

15%

41

62

70t≤150

620

720-890

15%

41

62

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate

 

Equivalent steel grade of NV F620

ABS

GL

LR

BV

CCS

NK

KR

RINA

AB/FQ63

GL-F620

LR/FH62

BV/F620

CCS/F620

K F63

R F63

RI/F620

 

To find more about shipbuilding steel plate, or inquiry from our gangsteel, please feel free to CLICK HERE to contact us.

Tags: DNV F620  NV F620  A620 steel grade  DNV Grade F620  F620 steel plate  NV F620 manufacturer  

0 Comments, 0 Trackbacks